Standard Method of Test for Accelerated Detection of Potentially Deleterious Expansion of Mortar Bars Due to Alkali-Silica Reaction
standard by American Association of State and Highway Transportation Officials, 2000
Description
This test method allows detection within 16 days of the potential for deleterious expansion of mortar bars due to the alkali-silica reaction.